Chemical Composition
0.28 to 0.35
%    
18 to 20
%    
64.4 to 71.3
%    (estimate)
1 to 1.7
%    
0.4
%    
8 to 11
%    
0.5
%  (maximum)  
1 to 1.7
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
296
MPa    
54
% strain    
189
   
 
Other Information
Hot rolled: 118,000 TS; 69,000 YS; 58 El; 55 RA; 216 HB; Heat treated: 103,000 TS; 43,000 YS; 54 El; 57 RA; 189 HB; For jet engine and gas turbine components; austenitic, heat resistant.
ALTEMP 19-19DL
 



No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®