Chemical Composition
0.015
%  (minimum)  
0.18
%    
98.1 to 98.2
%    (estimate)
1.3
%    
0.045
%  (maximum)  
0.045
%  (maximum)  
0.35
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
190
   
 
Other Information
Equivalent to Fr. A52-4; Sw. SS 14 2172; GBr. 4360-50D; ASTM A299/A537. Steel for general structural purposes. Soft annealed: 190 HB max; normalized to national/international standards for use.
DIRO-ST 52-3
 
Links
 