Chemical Composition
0.75
%    
0.8
%    
96.8
%    (estimate)
0.25
%    
1.25
%    
0.15
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
834 to 1430
MPa    
29 to 45
   
 
Other Information
Heat treated: 121,000-208,000 TS; 90,000-180,000 PL; 29-45 HRC; For brake dies, bushings, cams, shear blades, gears, set screws, swaging and forming dies, punches. Type L6, tough, oil hardening.
ECONO-2
 