Chemical Composition
93.7 to 94.1
%    (estimate)
5.5
%    
0.4 to 0.8
%    
Mg is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
290
MPa    
8
% strain    
 
Other Information
Extruded: 49,000 TS; 38,000 YS; 10 El. Heat treated: 51,000 TS; 42,000 YS; 8 El. For floor beams, aircraft structural members. High strength, good corrosion resistant. Shock resistant.