Chemical Composition
0.1
%    
0.003
%    
0.03
%  (maximum)  
9
%    
66.8 to 66.9
%    (estimate)
4.8
%    
18.5
%    
0.7
%    
0.02
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1930
MPa    
2000
MPa    
10
% strain    
 
Other Information
Annealed: 155,000 TS; 110,000 YS; 15 El; 70 RA; C 30 Rock. Maraged: 290,000 TS; 280,000 YS; 10 El; 55 RA; C 54 Rock. For missile components, rocket motor cases, engine parts, pressure vessels. High strength and fracture toughness. Maraging.
VAR STEEL GR. 280
 