Chemical Composition
0.04
%  (maximum)  
24.5 to 26.5
%    
2.7 to 3.3
%    
59.5 to 66.3
%    (estimate)
1
%  (maximum)  
1.7 to 2.3
%    
0.1 to 0.25
%    
4.7 to 6
%    
0.04
%  (maximum)  
0.04
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 