Chemical Composition
0.1 to 0.3
%    
0.08
%  (maximum)  
11.5 to 14
%    
83 to 88.4
%    (estimate)
1
%  (maximum)  
0.6
%  (maximum)  
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties