Chemical Composition
0.5
%  (maximum)  
98.7 to 99.2
%    (estimate)
0.8
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
276 to 414
MPa    
552 to 655
MPa    
18 to 28
% strain    
140 to 180
   
 
Other Information
Cast: 80,000-95,000 TS; 40,000-60,000 YP; 140-180 HB; 30-40 RA; 18-28 El. For general and structural applications, gears, housings. Weldable with caution. AISI 1040.
BIRDSBORO-40 CN
 