Chemical Composition
0.5
%  (maximum)  
2
%    
96.2 to 96.7
%    (estimate)
0.8
%    
0.5
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1000 to 1240
MPa    
1210 to 1450
MPa    
6 to 12
% strain    
290 to 350
   
 
Other Information
Heat treated: 175,000-210,000 TS; 145,000-180,000 YP; 6-12 El; 12-30 RA; 290-350 HB; For general and structural castings, gears, shafts, housings. Tough, shock resistant.
BIRDSBORO-45A7
 