Chemical Composition
0.07
%  (maximum)  
16 to 23
%    
65.9 to 77
%    (estimate)
7 to 11
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
483 to 586
MPa    
130 to 160
   
 
Other Information