Chemical Composition
0.35
%  (maximum)  
0.85
%    
95.7 to 96.1
%    (estimate)
0.75
%    
0.3
%    
2
%    
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
655 to 827
MPa    
827 to 1000
MPa    
14 to 20
% strain    
200 to 250
   
 
Other Information
Heat treated: 120,000-145,000 TS; 95,000-120,000 YP; 14-20 El; 30-40 RA; 200-250 HB; For general and structural castings, gears, shafting, housing. AISI 4330. Shock resistant.