Range attributes
170
   
0.53
%    
16
% strain    
97.7
%    (estimate)
0.9
%    
0.9
%    
359
MPa    
 
Logical attributes
Rod
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
Annealed: 96,000 TS; 52,000 YS; 16 El; 23 RA; 170 HB; For axles, gears, bolts, tie-rods, bushings; water hardened.
AMBO MSJ
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Annealed: 96,000 TS; 52,000 YS; 16 El; 23 RA; 170 HB; For axles, gears, bolts, tie-rods, bushings; water hardened.
 