Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Heat treated: 180,000-210,000 TS; 150,000-180,000 YP; 20-25 RA; 330-400 HB; For general and structural castings, shafts, gears, housings. AISI 4340. Shock resistant.
BIRDSBORO-40A3
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Heat treated: 180,000-210,000 TS; 150,000-180,000 YP; 20-25 RA; 330-400 HB; For general and structural castings, shafts, gears, housings. AISI 4340. Shock resistant.
 