Layout: No layout
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
Structural high-strength steel, AERMET 100 ALLOY (Carpenter Technology Corp.)
add data link
Range attributes
C (Carbon)
0.23
%
Co (Cobalt)
13.4
%
Cr (Chromium)
3.1
%
Elongation
14 to 16
% strain
Fe (Iron)
71
%
(estimate)
Mo (Molybdenum)
1.2
%
Ni (Nickel)
11.1
%
Ultimate Tensile Strength
1930 to 2000
MPa
Yield Strength
1690 to 1760
MPa
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Friday, September 12, 2014
Checked By
Tyler Flowers
Alloy Family
High-Strength Steel
Alloy Group
Structural
Balance
Fe (Iron)
Base Element
Fe (Iron)
Country
USA
Material Class
Ferrous Alloy
Source
Manufacturer's Datasheet
Specification Type
Manufacturer's Specification
Short text attributes
Composition Note_old
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Designation
AERMET 100 ALLOY
Similar UNS Number
K92580
Long text attributes
Composition Note
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Organization
Carpenter Technology Corp.
Hyperlink attributes
Online Source
Online Datasheet
Similar Alloys
Click here to find similar alloys
Further Information
Organizations
Carpenter Technology Corp.
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard