Layout: No layout
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
Copper, ANSONIA ALLOY C 18150 (Ansonia Copper & Brass, Inc.)
add data link
Range attributes
Cr (Chromium)
0.5 to 1.5
%
Cu (Copper)
98.9
%
Density
1360 to 2330
Mg/m^3
Others Total
0.3
%
Rockwell 15-T scale
0.321
Ultimate Tensile Strength
13 to 20
MPa
Yield Strength
65 to 85
MPa
Zr (Zirconium)
0.02 to 0.2
%
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Wednesday, September 10, 2014
Checked By
Tyler Flowers
Alloy Family
Copper
Alloy Group
Wrought copper
Alloy Sub-Group
Copper
Available forms
Rod
,
Strip
,
Strip
,
Wire
,
Wire
Base Element
Cu (Copper)
Country
USA
Material Class
Nonferrous Alloy
Source
Alloy Digest, ASM International
Specification Status
Active
Specification Type
Manufacturer's Specification
Short text attributes
Composition Note_old
Cu value includes Ag
Designation
ANSONIA ALLOY C 18150
Filing Code
Cu-828
Long text attributes
Composition Note
Cu value includes Ag
Organization
Ansonia Copper & Brass, Inc.
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Further Information
Organizations
Ansonia Copper & Brass, Inc.
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard