Layout: No layout
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
Low-Alloy (HSLA), DILLIDUR IMPACT (Dillinger Hutte GTS)
add data link
Range attributes
B (Boron)
0.005
% (maximum)
C (Carbon)
0.21
% (maximum)
Cr (Chromium)
1.5
% (maximum)
Density
3400 to 3820
Mg/m^3
Elongation
310 to 370
% strain
Fe (Iron)
92 to 100
%
(estimate)
Mn (Manganese)
1.8
% (maximum)
Mo (Molybdenum)
0.7
% (maximum)
Nb (Niobium)
0.04
% (maximum)
Others Total
3
% (maximum)
P (Phosphorus)
0.02
% (maximum)
Rockwell 15-T scale
0.28
S (Sulfur)
0.01
% (maximum)
Si (Silicon)
0.6
% (maximum)
Ultimate Tensile Strength
16
MPa
V (Vanadium)
0.09
% (maximum)
Yield Strength
131 to 142
MPa
Discrete attributes
~Checking Status
Verified - New record
Date Last Checked
Wednesday, September 10, 2014
Checked By
Tyler Flowers
Alloy Family
High-Strength Steel
Alloy Group
Low-alloy (HSLA)
Available forms
Plate
Balance
Fe (Iron)
Base Element
Fe (Iron)
Country
Germany
Material Class
Ferrous Alloy
Source
Alloy Digest, ASM International
Specification Status
Active
Specification Type
Manufacturer's Specification
Short text attributes
Composition Note_old
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Designation
DILLIDUR IMPACT
Filing Code
SA-681
Other elements_old
Ni, Cu
Long text attributes
Composition Note
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Organization
Dillinger Hutte GTS
Other elements
Ni, Cu
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Further Information
Organizations
Dillinger Hutte GTS
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard