Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Shielded metal-arc welding electrode for welding types 316 and 316L steels. 85,600 psi TS; 64,000 psi YS; 40% El.
EUTECTRODE E316L-16
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Shielded metal-arc welding electrode for welding types 316 and 316L steels. 85,600 psi TS; 64,000 psi YS; 40% El.
 