Range attributes
0.5
%  (maximum)  
1.05
%    
96.5 to 97
%    (estimate)
0.97
%    
0.25
%    
0.53
%    
0.21
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For arbors, axles, bolts, cams, gears, hubs, die liners; preheat treated at mill, shock and fatigue resistant.
NICHROLOY L
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For arbors, axles, bolts, cams, gears, hubs, die liners; preheat treated at mill, shock and fatigue resistant.
 