Range attributes
0.08
%    
4 to 6
%    
93.9 to 95.9
%    (estimate)
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For oil refinery equipment; corrosion resistant.
BETHADUR 502
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For oil refinery equipment; corrosion resistant.
 