Range attributes
Logical attributes
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Germany
For bearings, sleeves, liners; water hardened, wear resistant.
AMBO BW1
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For bearings, sleeves, liners; water hardened, wear resistant.
 
Hyperlink attributes
Integer attributes
ID
64480
232016
 