Range attributes
250
   
0.45
%    
1.5
%    
90.6
%    (estimate)
7.5
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Annealed: 250 HB; For tube mill piercer points; wear resistant.
B&W NO. 1440
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Annealed: 250 HB; For tube mill piercer points; wear resistant.
 
Hyperlink attributes
Integer attributes
ID
70084
232123
 
Further Information