Heat treated: 165,000 TS; 150,000 YS; 20 El; 59 RA; 280-300 HB; For shafts, pins, boring bars, piston rods; heat treated and stress-relieved bars, shock resistant.
ACCURLOY
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Heat treated: 165,000 TS; 150,000 YS; 20 El; 59 RA; 280-300 HB; For shafts, pins, boring bars, piston rods; heat treated and stress-relieved bars, shock resistant.
 