Range attributes
0.4
%    
4
%    
95.6
%    (estimate)
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
France
For hot work tools, shears; oil hardened.
POMPEY MKND
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For hot work tools, shears; oil hardened.
1 Ni+Mo
 
Hyperlink attributes