Range attributes
0.32
%    
5
%    
92.2
%    (estimate)
1.15
%    
1
%    
0.35
%    
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
France
For upsetters, punches, extrusion dies; oil or air hardened, hot work steel.
MOSTAR
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For upsetters, punches, extrusion dies; oil or air hardened, hot work steel.
 
Hyperlink attributes
Integer attributes
ID
139944
233368
 



No warranty is given for the accuracy of these data