Layout: No layout
View
Full datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
Nickel-chromium-molybdenum alloy steel, MANOIR ABRADUR 500 (Usines de A. Manoir, Pitres (Eure))
add data link
Range attributes
Brinell Hardness
32 to 280
C (Carbon)
0.4
%
Cr (Chromium)
1.4
%
Elongation
10 to 12
% strain
Fe (Iron)
94.3
%
(estimate)
Mo (Molybdenum)
0.4
%
Ni (Nickel)
3.5
%
Ultimate Tensile Strength
993 to 1080
MPa
Yield Strength
634 to 786
MPa
Logical attributes
Shaft
Yes
Discrete attributes
~Checking Status
Not verified - Original build
Date Last Checked
Thursday, October 17, 2013
Available forms
Shaft
Balance
Fe (Iron)
Base Element
Fe (Iron)
Country
France
Material Class
Ferrous Alloy
Source
Woldman's Engineering Alloys 9th ed. J. Frick Editor, ASM International 2000
Specification Status
Active
Specification Type
Manufacturer's Specification
Short text attributes
Composition Note_old
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Country*
France
Description_old
Heat treated: 144,000-156,000 psi TS; 92,000-114,000 psi YS; 10-12 El; 280-32 HB; For gears, shafts, countershafts, mining equipment; oil hardened, tough, shock resistant.
Designation
MANOIR ABRADUR 500
Long text attributes
Composition Note
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Description
Heat treated: 144,000-156,000 psi TS; 92,000-114,000 psi YS; 10-12 El; 280-32 HB; For gears, shafts, countershafts, mining equipment; oil hardened, tough, shock resistant.
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
ID
154798
Source ID
233580
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard