Range attributes
3
%    
95.7
%    (estimate)
1.3
%    
 
Logical attributes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
For rolls; cast iron.
GRAINLOY
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
For rolls; cast iron.
 