Cast: 80,000-95,000 TS; 50,000-65,000 YP; 22-30 El; 25-40 RA. For general and structural applications, gears, housings. AISI 1050.
BIRDSBORO-50 CN
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Cast: 80,000-95,000 TS; 50,000-65,000 YP; 22-30 El; 25-40 RA. For general and structural applications, gears, housings. AISI 1050.
 