Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Cast: 80,000-105,000 TS; 50,000-90,000 YS; 150-210 HB; 15-30 El; 30-40 RA. For general and structural applications, gears, housings. Good weldability.
BIRDSBORO-30A1
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Cast: 80,000-105,000 TS; 50,000-90,000 YS; 150-210 HB; 15-30 El; 30-40 RA. For general and structural applications, gears, housings. Good weldability.
 