Range attributes
0.18
%  (maximum)  
1.25
%    
20 to 30
% strain    
97.3 to 97.5
%    (estimate)
0.55
%    
0.5
%    
483 to 552
MPa    
0.2
%    
276 to 379
MPa    
 
Logical attributes
Yes
Yes
 
Discrete attributes
Short text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
USA
Cast: 70,000-80,000 TS; 40,000-55,000 YP; 20-30 El; 35-50 RA. For general and structural castings, shafting, gears, housings. Shock resistant.
BIRDSBORO-CRMO2 + V
 
Long text attributes
Fe is listed as a Balance element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Cast: 70,000-80,000 TS; 40,000-55,000 YP; 20-30 El; 35-50 RA. For general and structural castings, shafting, gears, housings. Shock resistant.
 