Range attributes
0.01
%    
99
%    
10
% strain    
1.00
%    
359
MPa    
 
Logical attributes
Bar
Yes
Yes
Rod
Yes
 
Discrete attributes
Short text attributes
USA
Leaded copper. Extruded and drawn rod, bar. For parts machined from rods, current carrying studs, nuts, bolts, parts for fine machining. Rod hard: 55000 psi TS; 52000 psi YS; 10 EL; 55 HRB; Elec. Conductivity 96% IACS. Free cutting high conductivity.
ANACONDA 1870
 
Long text attributes
Leaded copper. Extruded and drawn rod, bar. For parts machined from rods, current carrying studs, nuts, bolts, parts for fine machining. Rod hard: 55000 psi TS; 52000 psi YS; 10 EL; 55 HRB; Elec. Conductivity 96% IACS. Free cutting high conductivity.
 
Hyperlink attributes
Integer attributes
ID
57440
233125
 
Further Information



No warranty is given for the accuracy of these data