Chemical Composition
0.08
%  (maximum)  
17 to 19
%    
64.5 to 74
%    (estimate)
2
%  (maximum)  
0.5
%  (maximum)  
9 to 12
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
0.8
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
200
MPa    
500 to 730
MPa    
30 to 40
% strain    
190
 (maximum)  
 