Chemical Composition
0.04 to 0.1
%    
15 to 17
%    
65.8 to 72.7
%    (estimate)
1.5
%  (maximum)  
1
%  (maximum)  
12 to 14
%    
0.035
%  (maximum)  
0.015
%  (maximum)  
0.3 to 0.6
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
205
MPa    
510 to 690
MPa    
35
% strain    
 
Other Information