Chemical Composition
0.08
%  (maximum)  
16.5 to 18.5
%    
61.5 to 70.5
%    (estimate)
2
%  (maximum)  
2 to 2.5
%    
11 to 13.5
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
0.8
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
210
MPa    
500 to 730
MPa    
35
% strain    
190
 (maximum)  
 