Chemical Composition
0.04 to 0.08
%    
17 to 19
%    
66.8 to 75
%    (estimate)
2
%  (maximum)  
0.11
%  (maximum)  
8 to 11
%    
0.035
%  (maximum)  
0.015
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
185
MPa  (minimum)  
500 to 700
MPa    
40
% strain  (minimum)  
 
Other Information