Chemical Composition
0.08
%  (maximum)  
16 to 18
%    
79.9 to 84
%    (estimate)
1
%  (maximum)  
0.04
%  (maximum)  
0.015
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
240
MPa  (minimum)  
430
MPa  (minimum)  
20
% strain  (minimum)  
 
Other Information