Chemical Composition
0.07
%  (maximum)  
19.5 to 20.5
%    
66.7 to 70
%    (estimate)
1 to 1.5
%    
9.5 to 10.5
%    
0.025
%  (maximum)  
0.015
%  (maximum)  
0.7
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Other Information
Links