Chemical Composition
0.06
%  (maximum)  
17 to 19
%    
64.8 to 72
%    (estimate)
2
%  (maximum)  
0.11
%  (maximum)  
11 to 13
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
190
MPa    
500 to 700
MPa    
35 to 45
% strain    
215
   
 
Other Information
Links



No warranty is given for the accuracy of these data