Chemical Composition
0.05
%  (maximum)  
16.5 to 18.5
%    
62.3 to 70.5
%    (estimate)
2
%  (maximum)  
2.5 to 3
%    
0.11
%  (maximum)  
10.5 to 13
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1100
MPa  (maximum)  
20
% strain  (minimum)  
 