Layout: No layout
View
Summary datasheet
Printable datasheet
Show empty items
Record properties
Expand headings
Collapse headings
Expand all metadata
Collapse all metadata
Change layout
No layout
~Release Layout
Alloy Finder (Default)
Explore Chemical Composition
Explore Properties
Tools
Add to list
Copy to clipboard
Export to text file…
Export to Excel…
Find substitutes for this record
View related records
Watch data…
Watch this record
Bookmark
Units
Metric
CGS (Consistent)
FPS (Consistent)
IPS (Consistent)
SI (Consistent)
UK Imperial
US Customary
420 grades, X30Cr13, MSZ 4360 (X30Cr13, MSZ 4360 (QT))
add data link
Range attributes
C (Carbon)
0.26 to 0.35
%
Cr (Chromium)
12 to 14
%
Elongation
11
% strain
Fe (Iron)
83 to 87.7
%
(estimate)
Mn (Manganese)
1
% (maximum)
Ni (Nickel)
0.6
% (maximum)
P (Phosphorus)
0.045
% (maximum)
S (Sulfur)
0.03
% (maximum)
Si (Silicon)
1
% (maximum)
Ultimate Tensile Strength
800 to 1000
MPa
Yield Strength
600
MPa
Discrete attributes
~Checking Status
Not verified - Original build
Date Last Checked
Thursday, October 17, 2013
Alloy Family
High-Alloy Steel (Corrosion and Heat Resistant, Stainless, and Nickel Steels)
Alloy Group
Martensitic stainless steel
Alloy Sub-Group
420 grades
Available forms
Wrought
Base Element
Fe (Iron)
Country
Hungary
Material Class
Ferrous Alloy
Source
Worldwide Guide to Equivalent Irons and Steels, 5th ed. ASM International 2006
Specification Status
Active
Specification Type
Standard
Standards Body
MSZ (Hungary)
Short text attributes
Composition Note_old
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Country*
Hungary
Description_old
Corrosion resistant; 0-100 mm; QT
Designation
X30Cr13
Specification
MSZ 4360
Long text attributes
Composition Note
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
Description
Corrosion resistant; 0-100 mm; QT
Hyperlink attributes
Similar Alloys
Click here to find similar alloys
Integer attributes
Specification Year
1987
Further Information
Organizations
Magyar Szabvanyugyi Testulet (MSZT) (Hungarian Standards Institution)
No warranty is given for the accuracy of these data
Copyright © 2024 ASM International®
UNHANDLED ERROR!
View log for stack trace
Close
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch record
Add to list
Copy to clipboard
Watch folder
Download Excel Template
Add to list
Copy to clipboard
Export Data to Excel
Find substitutes for this record
Watch generic
Download Excel Template
Add to list
Copy to clipboard
Watch table
Download Excel Template
Add all results from this table to list
Copy all results from this table to clipboard
Watch table
Add to list
Copy to clipboard
Find substitutes for this record
Watch record
Add all to list
Copy all to clipboard
Add all to list
Copy all to clipboard