Chemical Composition
0.03
%  (maximum)  
17 to 19.5
%    
65.7 to 74.4
%    (estimate)
2
%  (maximum)  
0.12 to 0.22
%    
8.5 to 11.5
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
255
MPa    
540 to 740
MPa    
40
% strain    
 