0.03
%  (maximum)  
28 to 30
%    
0.8
%  (maximum)  
56.6 to 63.6
%    (estimate)
0.8 to 1.5
%    
1.5 to 2.6
%    
0.3 to 0.4
%    
5.8 to 7.5
%    
0.03
%  (maximum)  
0.015
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
550
MPa  (minimum)  
750 to 1050
MPa    
25
% strain  (minimum)  
310
 (maximum)  
 