Chemical Composition
0.16 to 0.25
%    
12 to 14
%    
83.2 to 87.8
%    (estimate)
1.5
%  (maximum)  
0.04
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
500
MPa    
700 to 850
MPa    
13
% strain    
 
Other Information