Chemical Composition
0.02
%  (maximum)  
19 to 21
%    
0.5 to 1.5
%    
42.7 to 50.4
%    (estimate)
1
%  (maximum)  
6 to 7
%    
0.15 to 0.25
%    
24 to 26
%    
0.03
%  (maximum)  
0.01
%  (maximum)  
0.5
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
1100
MPa  (maximum)  
20
% strain  (minimum)  
 
Other Information
Links