Chemical Composition
0.08 to 0.15
%    
12 to 14
%    
83.6 to 87.8
%    (estimate)
1
%  (maximum)  
0.04
%  (maximum)  
0.15 to 0.25
%    
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
450
MPa    
650 to 850
MPa    
12
% strain    
 
Other Information