Chemical Composition
0.15
%  (maximum)  
16 to 18
%    
70.8 to 78
%    (estimate)
2
%  (maximum)  
6 to 8
%    
0.045
%  (maximum)  
0.03
%  (maximum)  
1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
960
MPa  (minimum)  
1270
MPa  (minimum)  
4
% strain  (minimum)  
 
Other Information