Chemical Composition
0.3
%    
0.03
%  (maximum)  
13 to 15
%    
0.75 to 1.5
%    
56.1 to 66.7
%    (estimate)
2
%  (maximum)  
0.75 to 1.5
%    
13 to 17
%    
0.04
%  (maximum)  
0.02
%  (maximum)  
5.5 to 6.5
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
255
MPa  (minimum)  
540
MPa  (minimum)  
28
% strain  (minimum)  
 
Other Information