Chemical Composition
0.06
%  (maximum)  
0.2
%  (maximum)  
0.3
%  (maximum)  
0.35
%  (maximum)  
96.3 to 98.9
%    (estimate)
1 to 1.45
%    
0.25
%  (maximum)  
0.04
%  (maximum)  
0.5
%  (maximum)  
0.03
%  (maximum)  
0.01
%  (maximum)  
0.15 to 0.4
%    
0.05
%  (maximum)  
0.1
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
315
MPa  (minimum)  
435 to 605
MPa    
25
% strain  (minimum)  
235
 (maximum)  
 