Chemical Composition
7.75 to 8.75
%    
3.5 to 4.25
%    
73.6 to 77.7
%    (estimate)
9 to 10
%    
0.08
%  (maximum)  
0.08
%  (maximum)  
0.95 to 1.35
%    
1.15 to 1.85
%    
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 