Chemical Composition
0.18
%  (maximum)  
97.2 to 100
%    (estimate)
1.65
%  (maximum)  
0.02
%  (maximum)  
0.1
%  (maximum)  
0.025
%  (maximum)  
0.035
%  (maximum)  
0.6
%  (maximum)  
0.15
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
485
MPa  (minimum)  
550
MPa  (minimum)  
17
% strain  (minimum)  
 
Other Information
Links



No warranty is given for the accuracy of these data