Chemical Composition
0.08
%  (maximum)  
16 to 18
%    
62.1 to 72
%    (estimate)
2
%  (maximum)  
2 to 3
%    
10 to 14
%    
0.04
%  (maximum)  
0.03
%  (maximum)  
0.75
%  (maximum)  
Fe is listed as a Base element for this material, but its % value is not listed in the specification. The value shown is a calculated one.
 
Mechanical Properties
205
MPa  (minimum)  
515
MPa  (minimum)  
35
% strain  (minimum)  
90
 (maximum)  
 
Other Information
Links